1、由于横向液体扩散和不断地更新液膜,使效率大大提高。
2、在传质和传热过程中,优异的表面利用率,可降低填料层高度。
3、被美国蒸馏协会(FRI) 的测试证实为高性能散堆填料。
4、良好的机械机构提供了的散堆性能和最低的窝堆状。
5、NC-MNR直接替代广泛使用的Nutter Ring.
6、Size:NO.0.7,NO.1.0,NO.1.5,NO.2.0,NO.2.5,NO.3.0
NC Metal Nutter Ring (NC-MNR)
1、Efficiency enhanced by lateral liquid spreading and surface film renewal.
2、 Superior surface utilization in mass and heat transfer,allowing shorter packed bed heights.
3、A high performance random packing verified by tests conducted at Fractionation Research Institute (FRI).
4、Mechanical form provides maximum randomness with minimal nesting.
5、NC-MNR Direct replacement of the widely used Nutter Ring.
6、Size:NO.0.7,NO.1.0,NO.1.5,NO.2.0,NO.2.5,NO.3.0