手机版链接:https://m.trustexporter.com/cz12475426.htm
耐磨损 德国巴斯夫 TPU C70AW 抗撕裂 水解稳定 韧性好 挤出级聚醚 Elastollan® C70AWThermoplastic Polyurethane Elastomer (Polyester)BASF Corp. Thermoplastic Polyurethanes产品说明:Elastollan® C70AW is a polyester-based thermoplastic polyurethane (TPU) containing a plasticizer. It exhibits excellent abrasion resistance and toughness, good hydrolytic stability, good heat, oil, fuel and solvent resistance. It has excellent damping characteristics and outstanding resistance to tear propagation. Elastollan® C70AW is supplied uncolored in pellet form.物性信息:基本信息添加剂增塑剂特性抗溶剂性良好的撕裂强度良好耐磨损性耐热性,高韧性良好水解稳定外观无色加工方法挤出注射成型物理性能额定值单位制测试方法比重1.15g/cm³ASTM D792熔流率(熔体流动速率) (190°C/3.8 kg)10 到 30g/10 minASTM D1238硬度额定值单位制测试方法肖氏硬度 (邵氏 A)69ASTM D2240机械性能额定值单位制测试方法拉伸模量 (注塑)11.0MPaASTM D412弯曲模量 (注塑)13.1MPaASTM D790泰伯耐磨性40.0mgASTM D1044Abrasion - DIN20mm³DIN 53516热性能额定值单位制测试方法Softening Point - DMA89°C内部方法弹性体额定值单位制测试方法拉伸应力ASTM D412 ****应变4.14MPaASTM D412 300%应变10.3MPaASTM D412抗张强度27.6MPaASTM D412伸长率 (断裂)720%ASTM D412撕裂强度 177.1kN/mASTM D624压缩yongjiu变形ASTM D395B 23°C, 22 hr20%ASTM D395B 70°C, 22 hr45%ASTM D395B热性能额定值单位制测试方法玻璃转化温度-48.0°C内部方法维卡软化温度67.0°CASTM D1525注射额定值单位制建议的最大水分含量0.030%料筒后部温度170 到 210°C料筒中部温度170 到 210°C料筒前部温度170 到 210°C射嘴温度200 到 210°C挤出额定值单位制料筒1区温度140 到 175°C料筒3区温度140 到 175°C料筒5区温度140 到 175°C接头温度160 到 175°C口模温度165 到 170°C耐磨损 德国巴斯夫 TPU C70AW 抗撕裂 水解稳定 韧性好 挤出级聚醚