手机版链接:https://m.trustexporter.com/cz12494752.htm
POM 韩国可隆 TF304物性表机械性能测试条件测试方法测试结果单位拉伸强度Yield,23℃MPaASTM D63845.0拉伸伸长率Yield,23℃%ASTM D638弯曲模量23°CMPaASTM D7902100弯曲强度23°CMPaASTM D790IZOD缺口冲击强度23°CJ/mASTM D25635.0热性能测试条件测试方法测试结果单位热畸变温度0.45MPa,未退火°CASTM D6481561.8MPa,未退火°CASTM D648106线性热膨胀系数flowcm/cm/°CASTM D6960.00013电气性能测试条件测试方法测试结果单位表面电阻率ohmsASTM D257体积电阻率ohm·cmASTM D257电气强度kV/mmASTM D149介电常数ASTM D1503.70介质损耗因数1E+6 HzASTM D1500.0060基本性能测试条件测试方法测试结果单位密度g/cm³ASTM D7921.51熔体质量流动速率190℃/2.16kgg/10 minASTM D1238收缩率flow%ASTM D9551.8吸水率Equilibrium,23℃,60%rh%ASTM D5700.20洛氏硬度M-ScaleASTM D785其他性能测试条件测试方法测试结果单位阻燃等级UL 94HB