手机版链接:
https://m.trustexporter.com/cz12980479.htm
高分子量HDPE CHNA-8380韩国韩华---Hanwha CHNA-8380 is a high molecular weight, high density polyethylene(HDPE) insulation compound especially designed for high-speed wire insulating extrusion process. It provides excellent processability, environmental and thermal stress cracking resistance. It meets major international aging test specification for both solid and foam/skin insulation. It can be used for the full range of telephone cable insulation including air-core, jelly-filled and LAN cable (Cat. 5/5e).
Hanwha CHNA-8380是一种高分子量、高密度聚乙烯(HDPE)绝缘化合物,专为高速线材绝缘挤出工艺而设计。它具有优异的加工性能、环境和热应力抗裂性。它符合固体和泡沫/皮肤绝缘的主要国际老化试验规范。它可用于各种电话电缆绝缘,包括空心电缆、果冻填充电缆和LAN电缆(5/5e类)。
CHNA-8380的物理性能额定值单位制测试方法
密度 | 0.945 | g/cm³ | ASTM D1505 |
熔流率(熔体流动速率) (190°C/2.16 kg) | 0.70 | g/10 min | ASTM D1238 |
抗环境应力开裂 (50°C, 10% Igepal, F0) | > 1000 | hr | ASTM D1693 |
硬度额定值单位制测试方法
肖氏硬度 (邵氏 D, 1 秒) | 53 |
| ASTM D2240 |
机械性能额定值单位制测试方法
抗张强度 | 23.5 | MPa | ASTM D638 |
伸长率 (断裂) | 550 | % | ASTM D638 |
老化额定值单位制测试方法
Oven Aging (100°C) | 2.0 | day |
|
拉伸强度保持率 - 2 days (100°C) | > 90 | % | ASTM D638 |
伸长保持率 - 2 days (100°C) | > 90 | % | ASTM D638 |
热性能额定值单位制测试方法
耐热应力裂纹 | > 96 | hr | ASTM D2951 |
氧感应时间 - AI (200°C) | > 100 | min | ASTM D3895 |
脆化温度 | < -76.0 | °C | ASTM D746 |